Designing snap-fits and clips for 3d printing

Snap-fits and clips that don't break when 3d printed: orientation, arm length and thickness, fillets, retention angles and the right material.

· by Marius Krämer

in short

service
NCS-03 · design & print custom parts
key rule
The arm must flex along the layers, not across them
arm
Long and thin rather than short and thick; tapering towards the tip
root
With a fillet instead of a sharp corner
material
PETG or PC; PLA is often too brittle for clips
approach
Print and test several variants at once

how a snap-fit works

A snap-fit is a flexible arm with a hook. When the parts are pushed together, the arm bends aside, the hook slides over an edge and catches behind it. For that to work, the arm has to bend far enough without breaking and then return to its shape.

That's the difficulty in 3d printing: printed parts are much weaker across the layers than along them. A clip that works as an injection moulded part can snap the first time it's engaged if it's printed in the wrong orientation.

orientation decides

The arm of a snap-fit has to sit in the printer so that it flexes along the layers. In practice that usually means the arm lies flat on the build plate instead of standing upright. An arm printed upright bends right at the layer lines and breaks there.

If the whole part has to be oriented differently for other reasons, it can make sense to print the clip as a separate part and fit it. Tell us where on the part the clips sit; we orient the part accordingly.

arm, root and hook

length
A longer arm bends less to travel the same distance.
thickness
Thinner and longer rather than thick and short; a thick, short arm breaks.
taper
Let it get thinner towards the tip so the bending spreads over the whole arm.
root
A fillet where the arm meets the part, not a sharp corner where it tears off.
lead-in angle
A shallow slope on the front of the hook so the arm moves aside smoothly.
retention face
Steep for a fixed joint, shallower if it should come apart again.

which material

Snap-fits need a tough material that bends without breaking. PETG is usually the best choice, PC takes even more. PLA is stiff and brittle; PLA clips break easily, especially the first time they're engaged. Carbon fibre filaments are very stiff and so flex little, and TPU is too soft to hold securely.

test rather than calculate

The exact spring and holding force of a printed clip depends on material, settings and orientation. The quickest route is to test several variants with slightly different arm thickness or hook height in one print. The variant that goes together well and holds securely goes into the series.

If the clip will be opened often, design it on the soft side: an arm that only has to bend a little per assembly lasts many more cycles.

frequently asked

3 questions
Why do 3d printed clips break?
Usually because the arm flexes across the layers or is too short and thick. Printed lying flat, longer and with a fillet at the root, they hold much better.
Which material suits snap-fits?
PETG for most clips, PC for high loads. PLA is often too brittle for clips.
How often can a printed clip be opened?
It depends on how far the arm has to bend each time. The less it bends per assembly, the more cycles it lasts.
NCS-03 · design & print custom parts guide: 3d printed enclosures glossary: 3d printing terms explained ask about a design
get in touch

tell us about
the part.

send files, a sketch or the broken original. no file? describe the part in a few lines.